Pure PTFE Gasket£¬ Polytetrafluoroethylene Gasket

WL-G1600

 

Description

WL-G1600 is made by cutting PTFE stick, pipe and sheet into flat shape PTFE gasket, v shape PTFE gasket or valve annulus PTFE gasket. PTFE gasket has 100% PTFE structure. It can bear the most bitter chemical medium, and PTFE gasket has good anti-creeping performance. PTFE gasket is a replacement of asbestos, and it is anti-creeping, anti-cold-flow, anti-low-temerature.PTFE gasket has no pollution and is easy to install and replace. under small pre-stress force, it can bear great internal pressure even in a environment of changing pressure. It is the best suit the condition with rough and fragile flange and alternately-changing temperature.

 

Main Specification

Pressure

=<10MPa

Temperature

-180¡æ¡«260¡æ

PH Range

0-14

Density

2.1-2.3g/cm3

Size

OD=<2000mm(special size can be made as request)



 

Modified PTFE Gasket

WL-G1610

 

Description

As we know, PTFE gasket is anti-creeping, anti-cold-flow, anti-low-temerature and PTFE gasket has no pollution. If we add some more useful element into the PTFE, the compression resistance and high temperature resistance will be more perfect. For example, can add some fibreglass, graphite, bronze to improve the character of pure PTFE gasket. We have PTFE gasket reinforced with glass fibre, graphite PTFE gasket, reformative PTFE gasket, PTFE bronze gasket, ect.

PTFE Graphite-filled Gasket: PTFE(teflon) graphite-filled is synthetic material made of PTFE and grapphite. It has perfect compressibility, recovery and sealing capability. Compared with traditional PTFE, it improve the low-flow and creep properties. It is more durable than normal PTFE gasket and extend the maintenance period of flange. So PTFE(teflon) graphite is economical choice.

PTFE Glass-filled Gasket: It is stamps gaskets from virgin and glass-filled PTFE.PTFE glass-filled gasket resist virtually all acids and caustics; It has the lowest known coefficient of friction of any solid, and has excellent electrical insulating properties. It has a continuous service temperature range of minus 350F to 500F. It is the ideal material for use in the petrochemical and chemical processing industries, and because it is FDA compliant, it can be used in the food processing and pharmaceutical industries also.

It have a shrinkage rate of approximately 5%. Glass filled PTFE gaskets have a lower shrink rate, because the glass fiber filler makes them harder, so they require less compression to seal adequately.

 

Main Specification

Pressure)

=<16MPa

Temperature

-180¡æ-260¡æ

PH

0-14

Density

2.1-2.3g/cm3

Size

OD=<2000mm(special size is made as request)

 

Consulted Dimension

No.

Type

Standard

Type

Standard

1

WRF 10A

¦µ53¡Á¦µ18¡Á3t

WFF 10A

¦µ90¡Á¦µ18¡Á3t

2

WRF 15A

¦µ58¡Á¦µ22¡Á3t

WFF 15A

¦µ95¡Á¦µ22¡Á3t

3

WRF 20A

¦µ63¡Á¦µ28¡Á3t

WFF 20A

¦µ100¡Á¦µ28¡Á3t

4

WRF 25A

¦µ74¡Á¦µ35¡Á3t

WFF 25A

¦µ125¡Á¦µ35¡Á3t

5

WRF 32A

¦µ84¡Á¦µ43¡Á3t

WFF 32A

¦µ135¡Á¦µ43¡Á3t

6

WRF 40A

¦µ89¡Á¦µ49¡Á3t

WFF 40A

¦µ140¡Á¦µ49¡Á3t

7

WRF 50A

¦µ104¡Á¦µ61¡Á3t

WFF 50A

¦µ155¡Á¦µ61¡Á3t

8

WRF 65A

¦µ124¡Á¦µ77¡Á3t

WFF 65A

¦µ175¡Á¦µ77¡Á3t

9

WRF 80A

¦µ134¡Á¦µ90¡Á3t

WFF 80A

¦µ185¡Á¦µ90¡Á3t

10

WRF 90A

¦µ144¡Á¦µ102¡Á3t

WFF 90A

¦µ195¡Á¦µ102¡Á3t

11

WRF 100A

¦µ159¡Á¦µ115¡Á3t

WFF 100A

¦µ210¡Á¦µ115¡Á3t

12

WRF 125A

¦µ190¡Á¦µ141¡Á3t

WFF 125A

¦µ250¡Á¦µ141¡Á3t

13

WRF 150A

¦µ220¡Á¦µ167¡Á3t

WFF 150A

¦µ280¡Á¦µ167¡Á3t

14

WRF 200A

¦µ270¡Á¦µ218¡Á3t

WFF 175A

¦µ305¡Á¦µ192¡Á3t

15

WRF 225A

¦µ290¡Á¦µ244¡Á3t

WFF 200A

¦µ330¡Á¦µ218¡Á3t

16

WRF 250A

¦µ333¡Á¦µ270¡Á3t

WFF 250A

¦µ400¡Á¦µ270¡Á3t

17

WRF 300A

¦µ378¡Á¦µ321¡Á3t

WFF 300A

¦µ445¡Á¦µ321¡Á3t

18

WRF 350A

¦µ423¡Á¦µ359¡Á3t

WFF 350A

¦µ490¡Á¦µ359¡Á3t

19

WRF 400A

¦µ486¡Á¦µ410¡Á3t

WFF 400A

¦µ560¡Á¦µ410¡Á3t

20

WRF 450A

¦µ541¡Á¦µ460¡Á3t

WFF 450A

¦µ620¡Á¦µ460¡Á3t

21

WRF 500A

¦µ596¡Á¦µ513¡Á3t

WFF 500A

¦µ675¡Á¦µ513¡Á3t

22

WRF 600A

¦µ700¡Á¦µ615¡Á3t

WFF 550A

¦µ745¡Á¦µ564¡Á3t

 

 

 

¡¡

Warning: Gasket materials should never be recommended when both the temperature and the pressure are at the maximums listed.  Properties and applications shown are typical.  No application should be undertaken by anyone without independent study and evaluation for suitability. Never use more than one gasket in one flange joint, and never reuse a gasket.  Improper use or gasket selection could cause property damage and/or serious personal injury.  The data reported is a compilation of field testing, field service reports and/or in-house testing.  While the utmost care has gone into publishing the information contained herein, we assume no responsibility for errors.  The information and specifications  contained in this website are subject to change without notice. This revision cancels and obsoletes all previous editions.