Oval Ring Joint Gasket

WL-G1800

 

Description

Oval ring joint gasket is machined from solid metals in a variety of shapes. They are designed for high pressure, high temperature or highly corrosive applications. These basic shapes are used in pressures up to 10,000 psi. The dimensions are standardized and require specially grooved flanges. It is made of the most suitable material and shapes.

 

WL-G1800 ring joint gasket oval type is also called RTJ oval type. It is mechanically made from integral metal  include soft iron, SS304, SS316, carbon steel, SS321. It is mainly used in the joint part of high-temperature, high-pressure pipeline, tower, groove and heat exchanger, suitable for steam industry, petroleum industry and petro chemistry.

Standard£ºANSI B16.5-1973¡¢JPI-75-15-70¡¢GB 699¡¢GB1220¡¢JB755¡¢HG20633-9

Note£ºThe material of the oval ring jont gasket must be 15~20HB lower than the hardness of flange,and this kind of gaskets is non-recyclable.

The cross section

Mark

Tolerance(mm)

P

¡À0.177

W

¡À0.203

T

¡À0.39

 

Available Material

Material

Maximum Hardness

Temperature£¨ ¡æ £©

Abbreviations

Brinell

Rockwell¡°B¡±Grade

Soft Iron

90

56

-60¡«500

D

Low Carbon Steel

120

68

-40¡«540

S

SS304

160

83

-250¡«540

304

SS304L

160

83

-250¡«540

304L

SS316

160

83

-200¡«815

316

SS316L

160

83

-200¡«815

316L

SS321

160

83

-200¡«870

321

SS347

160

83

-200¡«870

347

SS410

170

86

-40¡«850

410

5Cr-0.5Mo

130

¡¡

-29¡«650

¡¡

Copper

80

¡¡

-100¡«315

¡¡

Aluminum

35

¡¡

-200¡«425

¡¡

Inconel 600

150

¡¡

-100¡«1095

¡¡

Incoloy 825

150

¡¡

-100¡«1095

¡¡

Monel 400

150

¡¡

-100¡«760

¡¡

Titanium

215

¡¡

-200¡«540

¡¡

Nickel 200 -

110

¡¡

200¡«760

¡¡

Hastelloy B2

230

¡¡

-100¡«1095

¡¡

Hastelloy C276

210

¡¡

-100¡«1095

¡¡

¡¡

Warning: Gasket materials should never be recommended when both the temperature and the pressure are at the maximums listed.  Properties and applications shown are typical.  No application should be undertaken by anyone without independent study and evaluation for suitability. Never use more than one gasket in one flange joint, and never reuse a gasket.  Improper use or gasket selection could cause property damage and/or serious personal injury.  The data reported is a compilation of field testing, field service reports and/or in-house testing.  While the utmost care has gone into publishing the information contained herein, we assume no responsibility for errors.  The information and specifications  contained in this website are subject to change without notice. This revision cancels and obsoletes all previous editions.